Hello again all!

First pulls of the resin castings for the 16" MK6 main gun turrents now out of the mold and cured. They turned out rather well! Let's take a look...........................

Here's all 6 range finders. The castings are on the right, master on the left. A lot more detail will be added to these soon. I try to keep the master pattern for these rather simple, a basic shape if you will, then add the finer detail stuff on the casting later on.

Another angle of the range finders here. I did minimal clean up on these castings, as well as the others!!

A forward view of the range finders. These are an angled up little mess and difficult to duplicate. I think I got them pretty close.

Here's the resin compound I used for the range finders. "Alumilite Super Plastic". This stuff is great for smaller parts. Cures in 3 minutes! You gotta be fast with the mix and pour of the resin! But, it's a small batch so this is easy. Mix for 60 seconds, then pour in the mold. I used this before on larger castings, but it cures too fast and get's extremly hot during the curing process on larger stuff like the turrent main bodies. It also can bubble, thus the reason for the rather simple mold for the RF's. Less nooks and crannies with this material is better. Cures so fast that air can get trapped in those little nooks. Then you got a bubble. Time consuming to fix. Keep it simple with this material. Read on............

In this photo resin has been poured into the main turrent body and the barbette mold and is in the curing stage. Note it is white in color. This is a different resin. Micro-Mark CR-600 High Performance Casting Resin. Two minute mix and pour time, but one hour cure. Water thin, this stuff mixes fast and pours really well, with NO bubbles. Since it cures slower, it doesn't get as hot as the other material. Great stuff! Part # 82057, from Micro-Mark.com.

Here's a closer shot of the resin pour into the turrent main body. Since these are a solid casting, they are pretty heavy!

Here's the material used for the main turrent body and the barbette. I used about 12 fl. oz. to pour the turrent body and the barbette.

One hour after the pour, here's the main turrent body. The resin has excellent reproduction qualities and is easy to work with. I did very little clean-up here on this casting. Came out pretty good, I am pleased with the results!!

Master pattern on the left, the casting on the right. The materials used here produced a nice, clean, bubble free casting. My master did help a little

Another view of the main turrent body. Master pattern on the left, casting on the right. The casting actually looks better than the master. Pay's off to take your time and do things right, as you can see. Since this resin dries white, the molded in details become rather obscured in the photos. You'll see the detail better after some paint is applied. I'll "scuff" all parts before primer coats.

A close up up the rear of the casting.

A close up of the turrent with the barbette assembly, below the turrent main body. As I said, lots of details to be installed yet, but the casting saves a lot of time. This is pretty much how I pulled the part out of the mold. Very minimal clean up. Took me 2 minutes!! Better than some of the other stuff for sale out there, if I may say so!

A good close up of the port side of the turrent & barbette. If you look close, you can see a couple of very tiny bubble marks. I'll fix those little goobers!! I'll now cast two more turrents and barbettes, then begin final detailing and paintwork on these. They should come out very well!! Stay tuned!! More to come!
On another note, CIC still recouperating and doing very well. It will take a while before she is back to herself. She is OK and says hello to all of you!
Again, thanks for all of your support! I continue on..................